Wall thickness influences printability and material properties: below 1.0mm may not print and risks damage; up to ~3mm has flexibility, and beyond this will be stiff. Thick walls may be hollowed out to avoid deformation during manufacturing, leaving the internal spaces full of unfused PA12 Nylon powder.
MINIMUM 1.0mm